Analysis- failed vibration tests
This is the one of the failed test, all the failed clay tests are because following reasons. 1: The thickness I tried 1mm, 2mm, 3mm and...
timetable from 24 May
24--31 make at least 150 pieces 31 May---2 June: low temperature fire 5--9:match video & QR code, high temperature fire 12--16 test...
Plan of summer show
3 group of sculpture hang---fish line size--- diameter 1.5m choice of sound what we think about sound same frequency you didn't...
Test- slip casting
I tested the different thickness and humidity, all of them are very hard to sound wave.
Analysis- about identify and marketing
Identify my self: 1 Website ----the ideal website mould is similar with http://nipponcolors.com I plan to separate the page from the...
Test- the larger size test
The larger size can not casting the sound wave details. I'm gonna come back to the small size and use speaker instead of vibration...
Analysis- tutorial with Maiko
1. Issues/subjects to be discussed: How can I develop the sound sculpture for the summer show. Is that necessary to make lager size? 2....
Analysis- Eliminated materials
liquid wax--cold too slow, the pattern can not be kept. when it cold down, the patterns between 40HZ to 100HZ are quite similar, ...
Test- pigment float on the water
The pattern can not identify sound. doesn't work.